Characterization of mechanical properties of hydroxyapatite–silicon–multi walled carbon nano tubes composite coatings synthesized by EPD on NiTi alloys for biomedical application. (June 2016)
- Record Type:
- Journal Article
- Title:
- Characterization of mechanical properties of hydroxyapatite–silicon–multi walled carbon nano tubes composite coatings synthesized by EPD on NiTi alloys for biomedical application. (June 2016)
- Main Title:
- Characterization of mechanical properties of hydroxyapatite–silicon–multi walled carbon nano tubes composite coatings synthesized by EPD on NiTi alloys for biomedical application
- Authors:
- Khalili, Vida
Khalil-Allafi, Jafar
Sengstock, Christina
Motemani, Yahya
Paulsen, Alexander
Frenzel, Jan
Eggeler, Gunther
Köller, Manfred - Abstract:
- Abstract: Release of Ni 1+ ions from NiTi alloy into tissue environment, biological response on the surface of NiTi and the allergic reaction of atopic people towards Ni are challengeable issues for biomedical application. In this study, composite coatings of hydroxyapatite–silicon multi walled carbon nano-tubes with 20 wt% Silicon and 1 wt% multi walled carbon nano-tubes of HA were deposited on a NiTi substrate using electrophoretic methods. The SEM images of coated samples exhibit a continuous and compact morphology for hydroxyapatite–silicon and hydroxyapatite–silicon–multi walled carbon nano-tubes coatings. Nano-indentation analysis on different locations of coatings represents the highest elastic modulus (45.8 GPa) for HA–Si–MWCNTs which is between the elastic modulus of NiTi substrate (66.5 GPa) and bone tissue (≈30 GPa). This results in decrease of stress gradient on coating–substrate–bone interfaces during performance. The results of nano-scratch analysis show the highest critical distance of delamination (2.5 mm) and normal load before failure (837 mN) as well as highest critical contact pressure for hydroxyapatite–silicon–multi walled carbon nano-tubes coating. The cell culture results show that human mesenchymal stem cells are able to adhere and proliferate on the pure hydroxyapatite and composite coatings. The presence of both silicon and multi walled carbon nano-tubes (CS3) in the hydroxyapatite coating induce more adherence of viable human mesenchymal stemAbstract: Release of Ni 1+ ions from NiTi alloy into tissue environment, biological response on the surface of NiTi and the allergic reaction of atopic people towards Ni are challengeable issues for biomedical application. In this study, composite coatings of hydroxyapatite–silicon multi walled carbon nano-tubes with 20 wt% Silicon and 1 wt% multi walled carbon nano-tubes of HA were deposited on a NiTi substrate using electrophoretic methods. The SEM images of coated samples exhibit a continuous and compact morphology for hydroxyapatite–silicon and hydroxyapatite–silicon–multi walled carbon nano-tubes coatings. Nano-indentation analysis on different locations of coatings represents the highest elastic modulus (45.8 GPa) for HA–Si–MWCNTs which is between the elastic modulus of NiTi substrate (66.5 GPa) and bone tissue (≈30 GPa). This results in decrease of stress gradient on coating–substrate–bone interfaces during performance. The results of nano-scratch analysis show the highest critical distance of delamination (2.5 mm) and normal load before failure (837 mN) as well as highest critical contact pressure for hydroxyapatite–silicon–multi walled carbon nano-tubes coating. The cell culture results show that human mesenchymal stem cells are able to adhere and proliferate on the pure hydroxyapatite and composite coatings. The presence of both silicon and multi walled carbon nano-tubes (CS3) in the hydroxyapatite coating induce more adherence of viable human mesenchymal stem cells in contrast to the HA coated samples with only silicon (CS2). These results make hydroxyapatite–silicon–multi walled carbon nano-tubes a promising composite coating for future bone implant application. Graphical abstract: Highlights: HA–Si–MWCNTs coating was fabricated on NiTi implant using electrophoretic deposition. HA–Si–MWCNTs coating has highest normal load before failure during scratch test. HA–Si–MWCNTs coating shows elastic modulus of 45.8 GPa between NiTi and bone tissue. Presence of both Si and MWCNTs in HA coating induce more adherence of viable hMSCs. … (more)
- Is Part Of:
- Journal of the mechanical behavior of biomedical materials. Volume 59(2016)
- Journal:
- Journal of the mechanical behavior of biomedical materials
- Issue:
- Volume 59(2016)
- Issue Display:
- Volume 59, Issue 2016 (2016)
- Year:
- 2016
- Volume:
- 59
- Issue:
- 2016
- Issue Sort Value:
- 2016-0059-2016-0000
- Page Start:
- 337
- Page End:
- 352
- Publication Date:
- 2016-06
- Subjects:
- Composite coating -- Nano-scratch -- Nano-indentation -- Electrophoretic deposition -- Hydroxyapatite
Biomedical materials -- Periodicals
Biomedical materials -- Mechanical properties -- Periodicals
Biomedical materials
Biomedical materials -- Mechanical properties
Periodicals
Electronic journals
610.28 - Journal URLs:
- http://www.sciencedirect.com/science/journal/17516161 ↗
http://www.elsevier.com/journals ↗ - DOI:
- 10.1016/j.jmbbm.2016.02.007 ↗
- Languages:
- English
- ISSNs:
- 1751-6161
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 5015.809000
British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 26867.xml