Numerical prediction and experimental analysis of the buckling loads of SMPC cylindrical shells under axial compression. (February 2023)
- Record Type:
- Journal Article
- Title:
- Numerical prediction and experimental analysis of the buckling loads of SMPC cylindrical shells under axial compression. (February 2023)
- Main Title:
- Numerical prediction and experimental analysis of the buckling loads of SMPC cylindrical shells under axial compression
- Authors:
- Zhao, Hanxing
Lan, Xin
Liu, Liwu
Liu, Yanju
Leng, Jinsong - Abstract:
- Abstract: The axial compressive buckling loads of shape memory polymer composite (SMPC) cylindrical shells are very sensitive to geometric imperfections and temperatures, but few studies have been conducted on this phenomenon. In this study, the buckling loads and geometric imperfection sensitivities of SMPC cylindrical shells at different temperatures are determined by means of numerical simulations and experimental analyses. The single perturbation displacement imperfection (SPDI), multiple perturbation displacement imperfection (MPDI) and linear buckling mode imperfection (LBMI) techniques are used to simulate the initial geometric imperfections and calculate the corresponding buckling loads and knock-down factors (KDFs) of SMPC cylindrical shells at different temperatures. In the experimental part, the [ 0 / 90 / ± 45 ] s SMPC cylindrical shells are manufactured through the autoclave molding process. The load-bearing capacities at different temperatures are tested and compared with the numerical results. The results demonstrate that the buckling loads of the SMPC cylindrical shell obtained by numerical techniques are sensitive to temperature, while the KDFs are insensitive to temperature. Meanwhile, results indicate that brittle fracture is the main failure mode instead of buckling at low temperature, so there is a risk when using any numerical technique to design SMPC cylindrical shells in low-temperature region. At high temperatures, the SPDI method overestimates theAbstract: The axial compressive buckling loads of shape memory polymer composite (SMPC) cylindrical shells are very sensitive to geometric imperfections and temperatures, but few studies have been conducted on this phenomenon. In this study, the buckling loads and geometric imperfection sensitivities of SMPC cylindrical shells at different temperatures are determined by means of numerical simulations and experimental analyses. The single perturbation displacement imperfection (SPDI), multiple perturbation displacement imperfection (MPDI) and linear buckling mode imperfection (LBMI) techniques are used to simulate the initial geometric imperfections and calculate the corresponding buckling loads and knock-down factors (KDFs) of SMPC cylindrical shells at different temperatures. In the experimental part, the [ 0 / 90 / ± 45 ] s SMPC cylindrical shells are manufactured through the autoclave molding process. The load-bearing capacities at different temperatures are tested and compared with the numerical results. The results demonstrate that the buckling loads of the SMPC cylindrical shell obtained by numerical techniques are sensitive to temperature, while the KDFs are insensitive to temperature. Meanwhile, results indicate that brittle fracture is the main failure mode instead of buckling at low temperature, so there is a risk when using any numerical technique to design SMPC cylindrical shells in low-temperature region. At high temperatures, the SPDI method overestimates the KDFs, while the KDFs calculated by the MPDI and LBMI techniques are in good agreement with the experimental results. However, only the LBMI method can distinguish the influence of temperature on the post-buckling patterns, and the corresponding post-buckling pattern is more consistent with the experiment. In addition, the shape-recovery properties and repeatability of the SMPC cylindrical shells are good. Highlights: The buckling loads of the SMPC cylindrical shell obtained by numerical techniques are sensitive to temperature, while the KDFs are insensitive to temperature. In the low-temperature region, the SMPC cylindrical shell is more prone to brittle fracture than buckling deformation during the axial compressive experiment. In the high-temperature region, the SMPC cylindrical shell buckles before being destroyed. An assumption of the potential application of SMPC cylindrical shells is proposed. … (more)
- Is Part Of:
- Thin-walled structures. Volume 183(2023)
- Journal:
- Thin-walled structures
- Issue:
- Volume 183(2023)
- Issue Display:
- Volume 183, Issue 2023 (2023)
- Year:
- 2023
- Volume:
- 183
- Issue:
- 2023
- Issue Sort Value:
- 2023-0183-2023-0000
- Page Start:
- Page End:
- Publication Date:
- 2023-02
- Subjects:
- SMPC -- Cylindrical shell -- KDF -- Buckling load -- Repeatability
Thin-walled structures -- Periodicals
690.1 - Journal URLs:
- http://www.sciencedirect.com/science/journal/02638231 ↗
http://www.elsevier.com/journals ↗ - DOI:
- 10.1016/j.tws.2022.110340 ↗
- Languages:
- English
- ISSNs:
- 0263-8231
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 8820.121000
British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 25668.xml