Effect of Moisture Absorption on Mode II Fracture Behavior of Fumed Silica Reinforced Hybrid Fiber Composite. Issue 16 (28th November 2022)
- Record Type:
- Journal Article
- Title:
- Effect of Moisture Absorption on Mode II Fracture Behavior of Fumed Silica Reinforced Hybrid Fiber Composite. Issue 16 (28th November 2022)
- Main Title:
- Effect of Moisture Absorption on Mode II Fracture Behavior of Fumed Silica Reinforced Hybrid Fiber Composite
- Authors:
- Maharana, Sunil Manohar
Pandit, Mihir Kumar
Pradhan, Arun Kumar - Abstract:
- ABSTRACT: This work aims to investigate the influence of water ingression on Mode II interlaminar fracture behavior of a fumed silica-reinforced jute-kevlar hybrid nanocomposite. Shear mode of failure is characterized by using End Notched Flexure (ENF) specimens. Thirteen different composites are prepared based on four layering sequences (i.e., Jute-Jute-Jute-Jute [JJJJ], Jute-Kevlar-Kevlar-Jute [JKKJ], Kevlar-Jute-Jute-Kevlar [KJJK], and Kevlar-Kevlar-Kevlar-Kevlar [KKKK]) and four nanofiller weight proportions (0, 1.5, 3, and 4.5%), with the aim of studying the impact of the layering sequence and nanofiller proportion. Initiation fracture toughness (GIIC init. ) is reported for dry and wet conditions of the composites using the Simple Beam Theory (SBT) data reduction method. Among the reported stacking sequences, the stacking sequence JKKJ possesses the highest fracture-resistant material in both dry and wet conditions because of the active involvement of the fiber and matrices at the interlaminar layer resulting from interlaminar crack propagation. The water-aged composite JKKJ with a 3% nanofiller weight proportion shows the highest initiation fracture toughness (GIIC init. ) value, 1811.4 J/m 2 . The composite with the stacking sequence JKKJ and 3% nanofiller weight proportion is recommended, which is proved to be the best Mode II fracture-resistant material under wet conditions among the reported composites.
- Is Part Of:
- Journal of natural fibers. Volume 19:Issue 16(2022)
- Journal:
- Journal of natural fibers
- Issue:
- Volume 19:Issue 16(2022)
- Issue Display:
- Volume 19, Issue 16 (2022)
- Year:
- 2022
- Volume:
- 19
- Issue:
- 16
- Issue Sort Value:
- 2022-0019-0016-0000
- Page Start:
- 12548
- Page End:
- 12564
- Publication Date:
- 2022-11-28
- Subjects:
- Interlaminar fracture toughness -- Jute -- fumed silica -- Kevlar -- Mode II -- nanocomposite
层间断裂韧性 -- 黄麻 -- 气相二氧化硅 -- 凯夫拉尔 -- 模式二 -- 纳米复合材料
Textile research -- Periodicals
Textile research
Periodicals
677.005 - Journal URLs:
- http://www.tandfonline.com/toc/wjnf20/current ↗
http://www.tandfonline.com/ ↗ - DOI:
- 10.1080/15440478.2022.2073315 ↗
- Languages:
- English
- ISSNs:
- 1544-0478
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 24466.xml