Ambient Storage Derived Surface Contamination of NCM811 and NCM111: Performance Implications and Mitigation Strategies. Issue 12 (1st January 2019)
- Record Type:
- Journal Article
- Title:
- Ambient Storage Derived Surface Contamination of NCM811 and NCM111: Performance Implications and Mitigation Strategies. Issue 12 (1st January 2019)
- Main Title:
- Ambient Storage Derived Surface Contamination of NCM811 and NCM111: Performance Implications and Mitigation Strategies
- Authors:
- Sicklinger, Johannes
Metzger, Michael
Beyer, Hans
Pritzl, Daniel
Gasteiger, Hubert A. - Abstract:
- Abstract : The quality of metal oxide-based battery active materials is compromised by surface contamination from storage and handling at ambient conditions. We present a detailed analysis of the true nature and the quantity of the surface contaminants on two different cathode active materials, the widely used LiNi1/3 Co1/3 Mn1/3 O2 (NCM111) and the Ni-rich LiNi0.8 Co0.1 Mn0.1 O2 (NCM811). We process these materials in three distinct conditions "wet" (excessive exposure to moisture), "dry" (standard drying of as-received materials), and "calcined" (heat-treatment of cathode powders). Surface contaminants are then quantified by thermogravimetric analysis coupled with mass spectrometry (TGA-MS), and their reactivity with an ethylene carbonate-based electrolyte is evaluated using on-line mass spectrometry (OMS). We demonstrate that not only the commonly assumed LiOH and Li2 CO3 residues account for NCM performance deterioration upon storage in moisture and CO2 containing atmosphere, but also basic transition metal hydroxides/carbonates formed on the material surface. Eventually, we showcase a thermal treatment that removes these transition metal based surface contaminants and leads to superior cycling stability.
- Is Part Of:
- Journal of the Electrochemical Society. Volume 166:Issue 12(2019)
- Journal:
- Journal of the Electrochemical Society
- Issue:
- Volume 166:Issue 12(2019)
- Issue Display:
- Volume 166, Issue 12 (2019)
- Year:
- 2019
- Volume:
- 166
- Issue:
- 12
- Issue Sort Value:
- 2019-0166-0012-0000
- Page Start:
- A2322
- Page End:
- A2335
- Publication Date:
- 2019-01-01
- Subjects:
- Batteries - Lithium -- ambient storage -- cathode active material -- surface contamination
Electrochemistry -- Periodicals
541.3705 - Journal URLs:
- https://iopscience.iop.org/journal/1945-7111?gclid=EAIaIQobChMI4Y-UmqGC7wIVFeDtCh0VQAo7EAAYASAAEgLW8_D_BwE ↗
- DOI:
- 10.1149/2.0011912jes ↗
- Languages:
- English
- ISSNs:
- 0013-4651
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library HMNTS - ELD Digital store
- Ingest File:
- 22730.xml