Al and Mg Co-Doping Towards Development of Air-Stable and Li-Ion Conducting Li-La-Zirconate Based Solid Electrolyte Exhibiting Low Electrode/Electrolyte Interfacial Resistance. Issue 12 (17th August 2020)
- Record Type:
- Journal Article
- Title:
- Al and Mg Co-Doping Towards Development of Air-Stable and Li-Ion Conducting Li-La-Zirconate Based Solid Electrolyte Exhibiting Low Electrode/Electrolyte Interfacial Resistance. Issue 12 (17th August 2020)
- Main Title:
- Al and Mg Co-Doping Towards Development of Air-Stable and Li-Ion Conducting Li-La-Zirconate Based Solid Electrolyte Exhibiting Low Electrode/Electrolyte Interfacial Resistance
- Authors:
- Kobi, Sushobhan
Amardeep,
Vyas, Akhilesh
Bhargava, Parag
Mukhopadhyay, Amartya - Abstract:
- Abstract : Air-stable solid electrolytes, possessing good Li-ion conductivity and facilitating low resistance at electrode/electrolyte interface, are essential towards facile development/handling of safe-cum-stable solid-state Li-ion batteries, possessing desired power densities. In this context, we report here the design and development of Al/Mg co-doped Li-La-zirconate (LLZO) based solid electrolytes that address the concerns associated with inferior air stability of Al-doped LLZO, while retaining Li-ion conductivity (∼4.7 × 10 −4 s cm −1 ) as good as that for similarly developed Al-doped LLZO and higher than that for Mg-doped counterpart. Doping as "little" as 0.1 mole of Mg-ion (per mole of LLZO), as for the optimized Al(0.2)/Mg(0.1) co-doped LLZO, is sufficient to impart long term phase and structural stability in air, unlike that for Al-doped LLZO. Accordingly, Li-ion conductivity of Al(0.2)/Mg(0.1) co-doped LLZO gets nearly retained even after air-exposure for 50 days, in contrast to lowering of conductivity for Al-doped LLZO by ∼3 orders of magnitude after 24 days. The influence of excellent air stability and Li-ion conductivity could be seen on the Li/LLZO interfacial resistance, with the Al(0.2)/Mg(0.1) co-doped LLZO possessing the lowest area specific resistance of ∼18 Ω cm 2 among those investigated, which is also among the lowest reported to-date, without any additional surface/interfacial engineering being done.
- Is Part Of:
- Journal of the Electrochemical Society. Volume 167:Issue 12(2020)
- Journal:
- Journal of the Electrochemical Society
- Issue:
- Volume 167:Issue 12(2020)
- Issue Display:
- Volume 167, Issue 12 (2020)
- Year:
- 2020
- Volume:
- 167
- Issue:
- 12
- Issue Sort Value:
- 2020-0167-0012-0000
- Page Start:
- Page End:
- Publication Date:
- 2020-08-17
- Subjects:
- Batteries Li-ion -- Solid-State Ionics -- Energy Storage
Electrochemistry -- Periodicals
541.3705 - Journal URLs:
- https://iopscience.iop.org/journal/1945-7111?gclid=EAIaIQobChMI4Y-UmqGC7wIVFeDtCh0VQAo7EAAYASAAEgLW8_D_BwE ↗
- DOI:
- 10.1149/1945-7111/abad66 ↗
- Languages:
- English
- ISSNs:
- 0013-4651
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library HMNTS - ELD Digital store
- Ingest File:
- 20923.xml