A new method to determine the synergistic effects of area ratio and microstructure on the galvanic corrosion of LAS A508/309 L/308 L SS dissimilar metals weld. (10th July 2021)
- Record Type:
- Journal Article
- Title:
- A new method to determine the synergistic effects of area ratio and microstructure on the galvanic corrosion of LAS A508/309 L/308 L SS dissimilar metals weld. (10th July 2021)
- Main Title:
- A new method to determine the synergistic effects of area ratio and microstructure on the galvanic corrosion of LAS A508/309 L/308 L SS dissimilar metals weld
- Authors:
- Okonkwo, Bright O.
Ming, Hongliang
Wang, Jianqiu
Han, En-Hou
Rahimi, Ehsan
Davoodi, Ali
Hosseinpour, Saman - Abstract:
- Graphical abstract: Highlights: Three conspicuous regions were identified in the A508 base metal. Galvanic corrosion occurred between the coupled dissimilar metal. Area ratio and microstructure played various roles in the galvanic interaction of the DMW. Synergy was observed between both factors studied on the galvanic interaction. MnS inclusion induced pitting was the most dangerous mechanism of corrosion. Abstract: The synergistic effects of area ratio and microstructure on the galvanic corrosion of A508/309 L/308 L dissimilar metals weld (DMW) are studied by a multi-analytical approach. It was demonstrated that decreasing the anode/cathode surface area ratio obviously enhances the corrosion rate of A508, both locally and globally. Deeper analyses of the AFM results enabled quantitative comparison of the corrosion behaviour of the different surface constituents. It was revealed that in the galvanic interaction of the DMW, the grain refined region corrodes most, followed by the partial grain refined region and base metal matrix of the A508, respectively. The electrochemical localization index ( LI ) estimation method and AFM analysis both confirmed the presence of a mixed (localized and uniform) corrosion phenomenon occurring on the surface of the A508 anode metal in the galvanic interaction of the dissimilar metals. Finally, the degree of synergism equation was utilized to describe the synergistic effects of anode/cathode area ratio and the microstructure of the samples onGraphical abstract: Highlights: Three conspicuous regions were identified in the A508 base metal. Galvanic corrosion occurred between the coupled dissimilar metal. Area ratio and microstructure played various roles in the galvanic interaction of the DMW. Synergy was observed between both factors studied on the galvanic interaction. MnS inclusion induced pitting was the most dangerous mechanism of corrosion. Abstract: The synergistic effects of area ratio and microstructure on the galvanic corrosion of A508/309 L/308 L dissimilar metals weld (DMW) are studied by a multi-analytical approach. It was demonstrated that decreasing the anode/cathode surface area ratio obviously enhances the corrosion rate of A508, both locally and globally. Deeper analyses of the AFM results enabled quantitative comparison of the corrosion behaviour of the different surface constituents. It was revealed that in the galvanic interaction of the DMW, the grain refined region corrodes most, followed by the partial grain refined region and base metal matrix of the A508, respectively. The electrochemical localization index ( LI ) estimation method and AFM analysis both confirmed the presence of a mixed (localized and uniform) corrosion phenomenon occurring on the surface of the A508 anode metal in the galvanic interaction of the dissimilar metals. Finally, the degree of synergism equation was utilized to describe the synergistic effects of anode/cathode area ratio and the microstructure of the samples on the galvanic corrosion of LAS A508/309L/308L SS DMW. … (more)
- Is Part Of:
- Journal of materials science & technology. Volume 78(2021)
- Journal:
- Journal of materials science & technology
- Issue:
- Volume 78(2021)
- Issue Display:
- Volume 78, Issue 2021 (2021)
- Year:
- 2021
- Volume:
- 78
- Issue:
- 2021
- Issue Sort Value:
- 2021-0078-2021-0000
- Page Start:
- 38
- Page End:
- 50
- Publication Date:
- 2021-07-10
- Subjects:
- Low alloy steel -- Stainless steel -- SEM -- AFM -- Galvanic corrosion -- Inclusion
Metals -- Periodicals
Materials science -- Periodicals
Materials science
Metals
Periodicals
620.1105 - Journal URLs:
- http://www.jmst.org/EN/volumn/home.shtml ↗
http://www.sciencedirect.com/science/journal/10050302 ↗
http://www.sciencedirect.com/ ↗ - DOI:
- 10.1016/j.jmst.2020.10.044 ↗
- Languages:
- English
- ISSNs:
- 1005-0302
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 16817.xml