Use of nanoprobes to identify iron-silicates in a glass/iron/argillite system in deep geological disposal. (September 2019)
- Record Type:
- Journal Article
- Title:
- Use of nanoprobes to identify iron-silicates in a glass/iron/argillite system in deep geological disposal. (September 2019)
- Main Title:
- Use of nanoprobes to identify iron-silicates in a glass/iron/argillite system in deep geological disposal
- Authors:
- Carrière, C.
Dillmann, P.
Foy, E.
Neff, D.
Dynes, J.J.
Linard, Y.
Michau, N.
Martin, C. - Abstract:
- Highlights: A glass/iron/claystone system was altered at 50 °C for 4.5 years in Andra's underground research laboratory in Bure, France. Creation of a new database of reference spectra obtained on iron-silicate end-members by STXM at Si K-edge. Multi-scale (macro-micro-nano) and multitechnical (SEM-EDX, μRaman, STXM and TEM) characterization to identify iron-silicate. Nanometric crystallized Fe(III)-rich smectites were detected in the glass alteration layer and in the iron corrosion products. Abstract: The understanding of glass alteration mechanisms in contact with iron is a major issue to study the long-term behavior of radioactive waste package in repository conditions. A glass/iron/claystone system was altered in contact with COx water at 50 °C for 4.5 years in Andra's underground research laboratory in Bure, France. Multiscale and multitechnical (SEM-EDX, μRaman, STXM and TEM) characterization of the system revealed the presence of nanometric crystalline Fe(III)-rich smectite, assimilated to nontronite, in the glass alteration layer and in corrosion products. These phyllosilicates were identified by STXM using a comparative approach with a database of reference spectra obtained on iron-silicate.
- Is Part Of:
- Corrosion science. Volume 158(2019)
- Journal:
- Corrosion science
- Issue:
- Volume 158(2019)
- Issue Display:
- Volume 158, Issue 2019 (2019)
- Year:
- 2019
- Volume:
- 158
- Issue:
- 2019
- Issue Sort Value:
- 2019-0158-2019-0000
- Page Start:
- Page End:
- Publication Date:
- 2019-09
- Subjects:
- SON68 nuclear glass -- Iron corrosion -- Glass alteration layer -- STXM -- Si K-edge -- Phyllosilicate
Corrosion and anti-corrosives -- Periodicals
620.11223 - Journal URLs:
- http://www.sciencedirect.com/science/journal/0010938X ↗
http://www.elsevier.com/journals ↗ - DOI:
- 10.1016/j.corsci.2019.108104 ↗
- Languages:
- English
- ISSNs:
- 0010-938X
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 3476.500000
British Library DSC - BLDSS-3PM
British Library STI - ELD Digital store - Ingest File:
- 16620.xml