Simultaneous improvement of mechanical and fire retardant properties of synthesised biodegradable guar gum-g-poly(butyl acrylate)/montmorillonite nanocomposite. (August 2018)
- Record Type:
- Journal Article
- Title:
- Simultaneous improvement of mechanical and fire retardant properties of synthesised biodegradable guar gum-g-poly(butyl acrylate)/montmorillonite nanocomposite. (August 2018)
- Main Title:
- Simultaneous improvement of mechanical and fire retardant properties of synthesised biodegradable guar gum-g-poly(butyl acrylate)/montmorillonite nanocomposite
- Authors:
- Jena, Dharmendra K.
Sahoo, Prafulla K. - Abstract:
- Abstract: A novel multicomponent biopolymer based nanocomposite was synthesised via graft copolymerization of butyl acrylate (BA) onto guar gum (GG) and montmorillonite (MMT) by using ammonium persulfate (APS) as a free radical initiator, in the presence of N, N′-methylene bisacrylamide (MBA) as a crosslinking agent. BA had been grafted onto GG chains and the participation of -OH groups of MMT in polymerization reaction was confirmed by FTIR spectra. XRD and TEM observations revealed that MMT was exfoliated and uniformly dispersed in guar gum-g-poly (butyl acrylate) (GG-g-PBA) matrix. The resultant nanocomposite showed remarkably improved thermal stability and mechanical properties. In addition, the excellent fire retardancy of nanocomposite results from the formation of compact and continuous char which not only hinders the migration of volatile decomposition products out of polymer matrix but also provides barrier for heat transfer evaluated by limiting oxygen index (LOI) and cone calorimetry test. The biodegradation of nanocomposite has been carried out for better commercialization and environmental concern. Highlights: Convert a cost effective biopolymer to a high performance fire retardant material by modification via grafting. An effort for reducing excessive consumption of petroleum resources and the environmental impact resulting from it. The nanocomposite was successfully synthesised by emulsifier free emulsion technique with excellent fire retardancy.
- Is Part Of:
- Polymer degradation and stability. Volume 154(2018)
- Journal:
- Polymer degradation and stability
- Issue:
- Volume 154(2018)
- Issue Display:
- Volume 154, Issue 2018 (2018)
- Year:
- 2018
- Volume:
- 154
- Issue:
- 2018
- Issue Sort Value:
- 2018-0154-2018-0000
- Page Start:
- 37
- Page End:
- 45
- Publication Date:
- 2018-08
- Subjects:
- Guar gum-g-poly(butyl acrylate) -- Biodegradation -- Nanocomposite -- Fire retadancy -- Mechanical property -- Thermal stability
Polymers -- Deterioration -- Periodicals
Stabilizing agents -- Periodicals
Polymères -- Dégradation -- Périodiques
Stabilisants -- Périodiques
668.9 - Journal URLs:
- http://www.sciencedirect.com/science/journal/01413910 ↗
http://www.elsevier.com/journals ↗ - DOI:
- 10.1016/j.polymdegradstab.2018.05.020 ↗
- Languages:
- English
- ISSNs:
- 0141-3910
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 6547.704700
British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 12836.xml