Low temperature effect on ATRP of styrene and substituted styrenes enabled by SaBOX ligand. (12th September 2019)
- Record Type:
- Journal Article
- Title:
- Low temperature effect on ATRP of styrene and substituted styrenes enabled by SaBOX ligand. (12th September 2019)
- Main Title:
- Low temperature effect on ATRP of styrene and substituted styrenes enabled by SaBOX ligand
- Authors:
- Wang, Xiao-Yan
Chen, Zhi-Hao
Sun, Xiu-Li
Tang, Yong - Abstract:
- Abstract: A series of side-armed bisoxazoline (SaBOX) ligands have been designed and prepared, which exhibited high activity under (SARA) ATRP conditions even at low temperatures. Notably, both polymerization rate and controllability on molecular weight (MW) were significantly improved by using 4-MeOSt as monomer instead of styrene under the conditions in this work, which is significantly different from the previous reports that only oligomers were produced in the conventional ATRP of 4-MeOSt due to the presence of cationic species. Systematic studies indicated that SaBOX ligand enabled the low polymerization temperature, which is necessary to suppress the cationic polymerization process and produce high MW polymers rather than oligomers during the ATRP of 4-MeOSt. Meanwhile, the highly active SaBOX ligand guaranteed the high polymerization rate and good controllability. Moreover, by employing these SaBOX ligands, the controlled ATRP of styrene and substituted styrenes could be successfully achieved at low temperatures (−30 °C–25 °C), producing polymers with molecular weights close to theoretical values and relatively narrow molecular weight distributions (Đs = 1.2–1.5). More notably, the triad syndiotacticity (rr) of polystyrene was gradually enhanced from 48% to 62% by lowering the polymerization temperature, which demonstrated that the stereospecificity could be tuned in ATRP of styrene for the first time. The improved syndiotacticity and the subdued side reactionsAbstract: A series of side-armed bisoxazoline (SaBOX) ligands have been designed and prepared, which exhibited high activity under (SARA) ATRP conditions even at low temperatures. Notably, both polymerization rate and controllability on molecular weight (MW) were significantly improved by using 4-MeOSt as monomer instead of styrene under the conditions in this work, which is significantly different from the previous reports that only oligomers were produced in the conventional ATRP of 4-MeOSt due to the presence of cationic species. Systematic studies indicated that SaBOX ligand enabled the low polymerization temperature, which is necessary to suppress the cationic polymerization process and produce high MW polymers rather than oligomers during the ATRP of 4-MeOSt. Meanwhile, the highly active SaBOX ligand guaranteed the high polymerization rate and good controllability. Moreover, by employing these SaBOX ligands, the controlled ATRP of styrene and substituted styrenes could be successfully achieved at low temperatures (−30 °C–25 °C), producing polymers with molecular weights close to theoretical values and relatively narrow molecular weight distributions (Đs = 1.2–1.5). More notably, the triad syndiotacticity (rr) of polystyrene was gradually enhanced from 48% to 62% by lowering the polymerization temperature, which demonstrated that the stereospecificity could be tuned in ATRP of styrene for the first time. The improved syndiotacticity and the subdued side reactions indicated the superiority and necessity of the polymerization at low temperature for ATRP in some aspects. Graphical abstract: Image 1 Highlights: Controlled ATRP of styrene type monomers were achieved at low temperatures. ATRP of 4-MeOSt provided polymers rather than oligomers. Stereospecificity of polystyrene was gradually enhanced by lowering the temperature. A series of novel SaBOX ligands exhibited high activity at low temperature. … (more)
- Is Part Of:
- Polymer. Volume 178(2019)
- Journal:
- Polymer
- Issue:
- Volume 178(2019)
- Issue Display:
- Volume 178, Issue 2019 (2019)
- Year:
- 2019
- Volume:
- 178
- Issue:
- 2019
- Issue Sort Value:
- 2019-0178-2019-0000
- Page Start:
- Page End:
- Publication Date:
- 2019-09-12
- Subjects:
- Ambient and low temperature ATRP -- Bisoxazoline (BOX) -- Styrene type monomers
Polymers -- Periodicals
Polymerization -- Periodicals
Polymères -- Périodiques
Polymérisation -- Périodiques
547.7 - Journal URLs:
- http://www.sciencedirect.com/science/journal/00323861 ↗
http://www.elsevier.com/journals ↗ - DOI:
- 10.1016/j.polymer.2019.121630 ↗
- Languages:
- English
- ISSNs:
- 0032-3861
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 6547.700000
British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 11624.xml