Surface mould growth on wooden claddings – effects of transient wetting, relative humidity, temperature and material properties. Issue 3 (4th May 2019)
- Record Type:
- Journal Article
- Title:
- Surface mould growth on wooden claddings – effects of transient wetting, relative humidity, temperature and material properties. Issue 3 (4th May 2019)
- Main Title:
- Surface mould growth on wooden claddings – effects of transient wetting, relative humidity, temperature and material properties
- Authors:
- Lie, Solrun Karlsen
Vestøl, Geir I.
Høibø, Olav
Gobakken, Lone Ross - Abstract:
- ABSTRACT: Effects of climatic factors and material properties on the development of surface mould growth on wooden claddings were investigated in a laboratory experiment. Specimens of aspen ( Populus tremula ), Siberian larch ( Larix Sibirica ), American white oak ( Querqus alba ), Scots pine ( Pinus sylvestris ), Norway spruce ( Picea abies ) and thermally modified pine were incubated in eight climatic chambers at specified wetting periods (2 or 4 h per day), relative humidity (58–86%) and temperature conditions (10–27°C). Surface mould growth was assessed weekly for 13 weeks, and the results were evaluated statistically using Generalized Estimating Equations logistic regression models. All tested climatic factors had significant effects on the mould growth, and there were significant differences between the materials. The ranking of the materials varied with temperature and over time. Aspen, pine sapwood and oak were overall most susceptible to mould growth, and thermally modified pine least susceptible. There were significant differences between sapwood and heartwood for pine and spruce. The effect of density was tested on the spruce heartwood material, but was not found to be significant. The results can be used to further develop prediction models for mould growth on wooden claddings.
- Is Part Of:
- Wood material science & engineering. Volume 14:Issue 3(2019)
- Journal:
- Wood material science & engineering
- Issue:
- Volume 14:Issue 3(2019)
- Issue Display:
- Volume 14, Issue 3 (2019)
- Year:
- 2019
- Volume:
- 14
- Issue:
- 3
- Issue Sort Value:
- 2019-0014-0003-0000
- Page Start:
- 129
- Page End:
- 141
- Publication Date:
- 2019-05-04
- Subjects:
- Wooden façades -- climate factors -- blue stain fungi -- pine -- spruce
Wood -- Periodicals
Wood products -- Periodicals
Building, Wooden -- Periodicals
624.184 - Journal URLs:
- http://www.tandf.co.uk/journals/titles/17480272.asp ↗
http://www.tandfonline.com/toc/swoo20/current ↗
http://www.tandfonline.com/ ↗ - DOI:
- 10.1080/17480272.2018.1424239 ↗
- Languages:
- English
- ISSNs:
- 1748-0272
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 9345.418200
British Library DSC - BLDSS-3PM
British Library STI - ELD Digital store - Ingest File:
- 9791.xml