Joining Ti3SiC2 MAX phase with 308 stainless steel and aluminum fillers by tungsten inert gas (TIG)-brazing process. Issue 1 (January 2016)
- Record Type:
- Journal Article
- Title:
- Joining Ti3SiC2 MAX phase with 308 stainless steel and aluminum fillers by tungsten inert gas (TIG)-brazing process. Issue 1 (January 2016)
- Main Title:
- Joining Ti3SiC2 MAX phase with 308 stainless steel and aluminum fillers by tungsten inert gas (TIG)-brazing process
- Authors:
- Hadji, Y.
Haddad, A.
Yahi, M.
Benamar, M.E.A
Miroud, D.
Sahraoui, T.
Hadji, M.
Barsoum, M.W. - Abstract:
- Abstract: Herein we report on the Tungsten Inert Gas (TIG) brazing of Ti3 SiC2 to 308 stainless steel and Al brazing fillers materials. The microstructures of the interfaces were investigated by scanning electron microscopy and energy dispersive spectrometry. Intensive interactions including dissolution and diffusion simultaneously occurred within the Ti3 SiC2 and at the Ti3 SiC2 /308 stainless steel interface during TIG-Brazing. The interfacial region between Ti3 SiC2 and 308 stainless steel filler is comprised of a decomposed Ti3 SiC2 zone, an interaction layer zone and a modified 308 stainless steel zone. When the Ti3 SiC2 comes into contact with the 308 SS molten filler during TIG-brazing, it starts decomposing into a TiC x +SiLiquid +Sigas, and simultaneously, deep penetration of the molten 308 SS into the Ti3 SiC2 occurred to form a complex bright phase containing [Fe, Cr, Ni, Ti, C, Si] and TiC x phase. The loss of Si is attributed to its evaporation during the TIG-brazing process. Thermally induced residual stress due to thermal expansion mismatches create interfacial cracks between the decomposed Ti3 SiC2 and the interaction layer zone. The phases that most likely form when Ti3 SiC2 is joined with Al brazed filler material are Al in which some Si is dissolved, TiAl3 and Ti4 AlC3 . No cracks were observed during TIG joining of Ti3 SiC2 with Al brazing filler material.
- Is Part Of:
- Ceramics international. Volume 42:Issue 1:Part B(2016)
- Journal:
- Ceramics international
- Issue:
- Volume 42:Issue 1:Part B(2016)
- Issue Display:
- Volume 42, Issue 1, Part 2 (2016)
- Year:
- 2016
- Volume:
- 42
- Issue:
- 1
- Part:
- 2
- Issue Sort Value:
- 2016-0042-0001-0002
- Page Start:
- 1026
- Page End:
- 1035
- Publication Date:
- 2016-01
- Subjects:
- MAX phase -- Joining -- TIG-Brazing -- Microstructure
Ceramics -- Periodicals
Céramique industrielle -- Périodiques
Ceramics
Periodicals
Electronic journals
666 - Journal URLs:
- http://www.sciencedirect.com/science/journal/02728842 ↗
http://www.elsevier.com/journals ↗ - DOI:
- 10.1016/j.ceramint.2015.09.026 ↗
- Languages:
- English
- ISSNs:
- 0272-8842
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 3119.015000
British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 7929.xml