Intergranular corrosion susceptibility of friction stir processed aluminium alloy 5083. (2018)
- Record Type:
- Journal Article
- Title:
- Intergranular corrosion susceptibility of friction stir processed aluminium alloy 5083. (2018)
- Main Title:
- Intergranular corrosion susceptibility of friction stir processed aluminium alloy 5083
- Authors:
- Vignesh, R. Vaira
Padmanaban, R. - Abstract:
- Abstract: The amalgamation of high strength and low density of aluminium alloys makes it suitable for light weight structural applications. Aluminium alloy AA5083 is prone to intergranular corrosion, when exposed to aggressive chloride containing marine environments. When aluminium alloy 5083 is exposed to marine environments, the continuous network of secondary phase particles present in the matrix reacts with the chloride ions and dissolves into the solution, creating new cites for corrosion. In addition to this phenomenon, secondary phase particles form galvanic couple with primary phase of the matrix, accelerating the corrosion. With an objective to improve the intergranular corrosion resistance, AA5083 was subjected to friction stir processing (FSP). FSP trials were conducted by varying the tool rotation speed, tool traverse speed and tool shoulder diameter, as per face centered central composite design. The intergranular corrosion susceptibility of friction stir processed AA5083 was studied by nitric acid mass loss test according to the ASTM G67-04 standard. Mathematical model was generated using linear – radial basis function and the model was used to study the effect of process parameters on the intergranular corrosion susceptibility of friction stir processed AA5083. The results indicate that FSP results in refinement of grain structure, dispersion and partial dissolution of secondary phase particles in the matrix, thereby reducing the intergranular corrosionAbstract: The amalgamation of high strength and low density of aluminium alloys makes it suitable for light weight structural applications. Aluminium alloy AA5083 is prone to intergranular corrosion, when exposed to aggressive chloride containing marine environments. When aluminium alloy 5083 is exposed to marine environments, the continuous network of secondary phase particles present in the matrix reacts with the chloride ions and dissolves into the solution, creating new cites for corrosion. In addition to this phenomenon, secondary phase particles form galvanic couple with primary phase of the matrix, accelerating the corrosion. With an objective to improve the intergranular corrosion resistance, AA5083 was subjected to friction stir processing (FSP). FSP trials were conducted by varying the tool rotation speed, tool traverse speed and tool shoulder diameter, as per face centered central composite design. The intergranular corrosion susceptibility of friction stir processed AA5083 was studied by nitric acid mass loss test according to the ASTM G67-04 standard. Mathematical model was generated using linear – radial basis function and the model was used to study the effect of process parameters on the intergranular corrosion susceptibility of friction stir processed AA5083. The results indicate that FSP results in refinement of grain structure, dispersion and partial dissolution of secondary phase particles in the matrix, thereby reducing the intergranular corrosion susceptibility of AA5083. … (more)
- Is Part Of:
- Materials today. Volume 5:Number 8(2018)Part 3
- Journal:
- Materials today
- Issue:
- Volume 5:Number 8(2018)Part 3
- Issue Display:
- Volume 5, Issue 8, Part 3 (2018)
- Year:
- 2018
- Volume:
- 5
- Issue:
- 8
- Part:
- 3
- Issue Sort Value:
- 2018-0005-0008-0003
- Page Start:
- 16443
- Page End:
- 16452
- Publication Date:
- 2018
- Subjects:
- Friction stir processing -- Aluminium alloy -- Central composite desing -- Corrosion -- Intergranular corrosion -- Radial basis function
Materials science -- Congresses -- Periodicals
620.1 - Journal URLs:
- http://www.sciencedirect.com/science/journal/22147853 ↗
http://www.sciencedirect.com/ ↗ - DOI:
- 10.1016/j.matpr.2018.05.143 ↗
- Languages:
- English
- ISSNs:
- 2214-7853
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 7832.xml