Durability of a low shrinkage TEGDMA/HEMA-free resin composite system in Class II restorations. A 6-year follow up. Issue 8 (August 2017)
- Record Type:
- Journal Article
- Title:
- Durability of a low shrinkage TEGDMA/HEMA-free resin composite system in Class II restorations. A 6-year follow up. Issue 8 (August 2017)
- Main Title:
- Durability of a low shrinkage TEGDMA/HEMA-free resin composite system in Class II restorations. A 6-year follow up
- Authors:
- van Dijken, Jan W.V.
Pallesen, Ulla - Abstract:
- Abstract: Objective: The objective of this randomized controlled prospective trial was to evaluate the durability of a low shrinkage and TEGDMA/HEMA-free resin composite system in posterior restorations in a 6-year follow up. Methods: 139 Class II restorations were placed in 67 patients with a mean age of 53 years (range 29–82). Each participant received at random two, as similar as possible, Class II restorations. In the first cavity of each pair the TEGDMA/HEMA-free resin composite system was placed with its 3-step etch-and-rinse adhesive (cmf-els). In the second cavity a 1-step HEMA-free self-etch adhesive was used (AdheSe One F). The restorations were evaluated using slightly modified USPHS criteria at baseline and then yearly during 6 years. Caries risk and parafunctional habits of the participants were estimated. Results: Three molar teeth showed mild post-operative sensitivity during 3 weeks for temperature changes and occlusal forces. After 6 years, 134 Class II restorations were evaluated. Twenty-one restorations, 8 cmf-els (11.4%) and 13 ASE-els (20%) failed during the 6 years (p < 0.0001). The annual failure rates were 1.9% and 3.3%, respectively. The main reasons for failure were fracture followed by recurrent caries. Most fractures and all caries lesions were found in high risk participants. Significance: The Class II resin composite restorations performed with the new TEGDMA/HEMA-free low shrinkage resin composite system showed good durability over six years.
- Is Part Of:
- Dental materials. Volume 33:Issue 8(2017)
- Journal:
- Dental materials
- Issue:
- Volume 33:Issue 8(2017)
- Issue Display:
- Volume 33, Issue 8 (2017)
- Year:
- 2017
- Volume:
- 33
- Issue:
- 8
- Issue Sort Value:
- 2017-0033-0008-0000
- Page Start:
- 944
- Page End:
- 953
- Publication Date:
- 2017-08
- Subjects:
- Adhesive -- Clinical -- HEMA -- Low shrinkage -- Posterior -- Resin composite -- TEGDMA
Dentistry -- Periodicals
Dental materials -- Periodicals
617.695 - Journal URLs:
- http://www.elsevier.com/journals ↗
http://www.sciencedirect.com/science/journal/01095641/ ↗ - DOI:
- 10.1016/j.dental.2017.04.021 ↗
- Languages:
- English
- ISSNs:
- 0109-5641
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 3553.365800
British Library DSC - BLDSS-3PM
British Library STI - ELD Digital store - Ingest File:
- 7009.xml