Cyclic-tearing behaviour and J–R curves of Indian NPP pipes under displacement-controlled cyclic loading. (August 2015)
- Record Type:
- Journal Article
- Title:
- Cyclic-tearing behaviour and J–R curves of Indian NPP pipes under displacement-controlled cyclic loading. (August 2015)
- Main Title:
- Cyclic-tearing behaviour and J–R curves of Indian NPP pipes under displacement-controlled cyclic loading
- Authors:
- Gupta, Suneel K.
Bhasin, V.
Chattopadhyay, J.
Ghosh, A.K.
Singh, R.K. - Abstract:
- Abstract: Currently the ductile fracture assessment of cracked pipes, under earthquake loading, is based on the monotonic J – R curve where the earthquake load is considered as a one-time applied load monotonically increasing to its maximum magnitude. The cyclic nature of earthquake load and associated cyclic-tearing damage (or cyclic J – R curve) is not explicitly considered. A series of cyclic-tearing and monotonic fracture tests is performed on circumferential through-wall-cracked pipes and pipe welds (five material categories) which are used in Indian Nuclear Power Plants (NPPs) piping system. The fracture behaviour of these pipes under cyclic loading vis-à-vis monotonic loading has been studied. The cyclic J – R curves of all material categories are significantly lower than the monotonic J – R curves and found strongly dependent on the applied load-history. Hence, cyclic J – R curve shall be evaluated for the load-history which is consistent with plant site (anticipated seismic loading), piping system layout and the crack location. The maximum moment observed during cyclic loading test is lower by a small to moderate amount than that obtained in the monotonic fracture tests on identical pipe. A relation has been obtained for cracked pipes which assesses if large crack growth/tearing would take place under displacement-controlled cyclic loading. Highlights: Cyclic/monotonic fracture pipe tests were conducted to understand cyclic fracture. Pipe fracture behaviour underAbstract: Currently the ductile fracture assessment of cracked pipes, under earthquake loading, is based on the monotonic J – R curve where the earthquake load is considered as a one-time applied load monotonically increasing to its maximum magnitude. The cyclic nature of earthquake load and associated cyclic-tearing damage (or cyclic J – R curve) is not explicitly considered. A series of cyclic-tearing and monotonic fracture tests is performed on circumferential through-wall-cracked pipes and pipe welds (five material categories) which are used in Indian Nuclear Power Plants (NPPs) piping system. The fracture behaviour of these pipes under cyclic loading vis-à-vis monotonic loading has been studied. The cyclic J – R curves of all material categories are significantly lower than the monotonic J – R curves and found strongly dependent on the applied load-history. Hence, cyclic J – R curve shall be evaluated for the load-history which is consistent with plant site (anticipated seismic loading), piping system layout and the crack location. The maximum moment observed during cyclic loading test is lower by a small to moderate amount than that obtained in the monotonic fracture tests on identical pipe. A relation has been obtained for cracked pipes which assesses if large crack growth/tearing would take place under displacement-controlled cyclic loading. Highlights: Cyclic/monotonic fracture pipe tests were conducted to understand cyclic fracture. Pipe fracture behaviour under displacement controlled cyclic loading studied. Cyclic J-R evaluated on 5 different material categories of Indian NPPs pipes. Relation developed to assesses if the cyclic loading cause large crack growth. … (more)
- Is Part Of:
- International journal of pressure vessels and piping. Volume 132/133(2015)
- Journal:
- International journal of pressure vessels and piping
- Issue:
- Volume 132/133(2015)
- Issue Display:
- Volume 132, Issue 2015 (2015)
- Year:
- 2015
- Volume:
- 132
- Issue:
- 2015
- Issue Sort Value:
- 2015-0132-2015-0000
- Page Start:
- 72
- Page End:
- 86
- Publication Date:
- 2015-08
- Subjects:
- Cyclic-tearing -- Cyclic J−R curve -- Leak−before−break (LBB) -- Crack growth -- Pipe
Pressure vessels -- Periodicals
Pipe -- Periodicals
Récipients sous pression -- Périodiques
Tuyaux -- Périodiques
Pipe
Pressure vessels
Periodicals
681.76041 - Journal URLs:
- http://www.sciencedirect.com/science/journal/03080161 ↗
http://www.elsevier.com/journals ↗ - DOI:
- 10.1016/j.ijpvp.2015.06.002 ↗
- Languages:
- English
- ISSNs:
- 0308-0161
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 4542.483000
British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 4938.xml