Degradation profiles of biodegradable plastic films by biodegradable plastic-degrading enzymes from the yeast Pseudozyma antarctica and the fungus Paraphoma sp. B47-9. (July 2017)
- Record Type:
- Journal Article
- Title:
- Degradation profiles of biodegradable plastic films by biodegradable plastic-degrading enzymes from the yeast Pseudozyma antarctica and the fungus Paraphoma sp. B47-9. (July 2017)
- Main Title:
- Degradation profiles of biodegradable plastic films by biodegradable plastic-degrading enzymes from the yeast Pseudozyma antarctica and the fungus Paraphoma sp. B47-9
- Authors:
- Sato, Shun
Saika, Azusa
Shinozaki, Yukiko
Watanabe, Takashi
Suzuki, Ken
Sameshima-Yamashita, Yuka
Fukuoka, Tokuma
Habe, Hiroshi
Morita, Tomotake
Kitamoto, Hiroko - Abstract:
- Abstract: Esterases from the yeast Pseudozyma antarctica (PaE) and the fungus Paraphoma sp. B47-9 (PCLE) can degrade biodegradable plastics (Shinozaki et al., 2013; Suzuki et al., 2014). The degradation profiles of plastic films composed of poly(butylene succinate), poly(butylene succinate- co -adipate), or poly(butylene adipate) by these enzymes were characterized by liquid chromatography-mass spectroscopy in terms of the molecular structures and molecular weights of the degradation products. Monomers and oligomers with molecular weights corresponding to dimers to octamers were identified as products of degradation by PaE in an aqueous reaction solution, irrespective of the type of biodegradable plastic film. Size-exclusion chromatography indicated that the number-average molecular weight of degraded films decreased with reaction time, suggesting that PaE degraded polyester films randomly into monomer units (endo-type degradation). PCLE also degraded polyester films randomly into monomer units, albeit more slowly than did PaE.
- Is Part Of:
- Polymer degradation and stability. Volume 141(2017)
- Journal:
- Polymer degradation and stability
- Issue:
- Volume 141(2017)
- Issue Display:
- Volume 141, Issue 2017 (2017)
- Year:
- 2017
- Volume:
- 141
- Issue:
- 2017
- Issue Sort Value:
- 2017-0141-2017-0000
- Page Start:
- 26
- Page End:
- 32
- Publication Date:
- 2017-07
- Subjects:
- Biodegradable -- Biodegradable plastics -- Pseudozyma antarctica -- Polyester hydrolase
Polymers -- Deterioration -- Periodicals
Stabilizing agents -- Periodicals
Polymères -- Dégradation -- Périodiques
Stabilisants -- Périodiques
668.9 - Journal URLs:
- http://www.sciencedirect.com/science/journal/01413910 ↗
http://www.elsevier.com/journals ↗ - DOI:
- 10.1016/j.polymdegradstab.2017.05.007 ↗
- Languages:
- English
- ISSNs:
- 0141-3910
- Deposit Type:
- Legaldeposit
- View Content:
- Available online (eLD content is only available in our Reading Rooms) ↗
- Physical Locations:
- British Library DSC - 6547.704700
British Library DSC - BLDSS-3PM
British Library HMNTS - ELD Digital store - Ingest File:
- 1958.xml