1. Shock-induced deformation twinning and softening in magnesium single crystals. (September 2020) Authors: Flanagan, Tyler J.; Vijayan, Sriram; Galitskiy, Sergey; Davis, Jacob; Bedard, Benjamin A.; Williams, Cyril L.; Dongare, Avinash M.; Aindow, Mark; Lee, Seok-Woo Journal: Materials & design Issue: Volume 194(2020) Page Start: Record Type: Journal Article View Content: Available online (eLD content is only available in our Reading Rooms) ↗