1. Changes in the Diffusion Coefficient of Rhenium in a New Type of Nickel‐Based Single‐Crystal Superalloy during Homogenization. Issue 4 (19th December 2019) Authors: Li, Yiling; Jia, Zhihong; Tang, Wei; Liang, Xiangfeng; Xu, Weitai; Zhao, Yutao Journal: Advanced engineering materials Issue: Volume 22:Issue 4(2020) Page Start: n/a Record Type: Journal Article View Content: Available online (eLD content is only available in our Reading Rooms) ↗